dc.creatorOLIVEIRA, Andressa Restani-
dc.creator.Latteshttp://lattes.cnpq.br/7583801058368978por
dc.contributor.advisor1Logar, Graziela Ávila Galhano-
dc.contributor.advisor1Latteshttp://lattes.cnpq.br/1681806064511416por
dc.contributor.advisor-co1Marocho, Susana Maria Salazar-
dc.contributor.advisor-co1Latteshttp://lattes.cnpq.br/9767390769588781por
dc.contributor.referee1Catelan, Anderson-
dc.contributor.referee1Latteshttp://lattes.cnpq.br/4629404319391359por
dc.contributor.referee2Marinho, Renata Marques de Melo-
dc.contributor.referee2Latteshttp://lattes.cnpq.br/3290027572731981por
dc.date.accessioned2019-10-15T19:03:00Z-
dc.date.issued2019-08-29-
dc.identifier.citationOLIVEIRA, Andressa Restani. Caracterização topográfica e mecânica de laminados cerâmicos com diferentes reduçōes incisais. 2019. Dissertação (Mestrado em Odontologia) - Universidade do Oeste Paulista, Presidente Prudente, 2019.por
dc.identifier.urihttp://bdtd.unoeste.br:8080/jspui/handle/jspui/1202-
dc.description.resumoAs propriedades mecânicas das cerâmicas estão diretamente relacionadas ao sucesso clínico dos laminados cerâmicos. Assim, objetivo deste estudo foi avaliar a tensão residual, dureza, efeito do polimento e determinar carga de fratura para laminados fabricados a partir de duas cerâmicas vítreas sobre diferentes reduçōes incisais (1 mm e 4 mm). Foram fabricados 52 laminados em cerâmica feldspática (FE) e silicato de lítio reforçado com zircônia (SZ), e divididos em 4 grupos (n = 13): FE1 - com redução incisal de 1 mm; FE4 - com redução incisal de 4 mm; SZ1 com redução incisal de 1 mm; SZ4 - com redução incisal de 4 mm. Os laminados foram obtidos através do método de desenho e manufatura assistidos por computador e cimentados em incisivos centrais superiores humanos. Todos os espécimes foram analisados antes e após o polimento em microscópio óptico e a rugosidade superficial foi medida pelo rugosímetro. Utilizou-se o método de indentação para estabelecer tensão residual e dureza Vickers e o ensaio de compressão foi realizado para determinação da carga de fratura. Depois de fraturados, a análise fractográfica dos espécimes foi realizada em microscópio óptico e eletrônico de varredura. Para rugosidade, o teste de Tukey foi aplicado para o material cerâmico e o teste de Mann-Whitney para o antes e depois do polimento. Para o ensaio de compressão utilizou-se ANOVA dois fatores e pós teste de Tukey. Para as demais análises foi aplicado o teste t de Student. A rugosidade diminuiu significativamente após o polimento (P < 0,001), enquanto a tensão residual (P = 0,722) e a dureza (P = 0,782) foram estatisticamente semelhantes para ambos os materiais. O tamanho de redução incisal apresentou efeito significativo na carga de fratura (P = 0,020). Trincas imperceptiveis em inspeção visual podem ser visualizadas quando observadas em microscopio óptico. A tensão residual e dureza foram similares para SZ e FE. O polimento diminuiu a rugosidade superficial das cerâmicas e pode aumentar o tamanho das trincas. A redução incisal no preparo (1 mm e 4 mm) para laminados cerâmicos apresentou diferentes valores de resistência à fratura, sendo que menores reduções incisais alcançaram valores mais altos de carga de fratura.por
dc.description.abstractThe mechanical properties of ceramics are directly related to the clinical success of ceramic veneers. Thus, the objective of this study was to evaluate the residual stress, hardness, surface roughness and to determine fracture load for veneers made from two glass- ceramics with different incisal reductions (1 mm and 4 mm). Fifty-two specimens of feldspar ceramic (FE) and zirconia-reinforced lithium silicate (SZ) veneers were prepared and divided into 4 groups (n = 13): FE1 - with 1 mm incisal reduction; FE4 - with 4 mm incisal reduction; SZ1 - with 1 mm incisal reduction; SZ4 - with 4 mm incisal reduction. The veneers were obtained through the computer- aided design and manufacturing method and cemented in human upper central incisors. All specimens were analyzed before and after polishing using an optical microscope and surface roughness were measured by the roughness meter. The indentation method was used to measure the residual stress and Vickers hardness and the compression test was performed to determine the fracture load. After fracturing, the fractographic analysis of the specimens was performed using optical and scanning electron microscopes. For roughness, the Tukey test was applied for the ceramic material and the Mann-Whitney test for before and after polishing. For the compression test, two-way ANOVA and Tukey post-test were used. For the other test, the Student’s t test was applied. The surface roughness decreased significantly after polishing (P <0.001), while residual stress (P = 0.722) and hardness (P = 0.782) were statistically similar for both materials. The size of the incisal reduction had a significant effect on fracture load (P = 0.020). Cracks imperceptible to visual inspection can be viewed when observed under optical microscopy. Residual stress and hardness were similar for SZ and FE. Polishing decreases the surface roughness of ceramics and can increase the size of the cracks. The incisal reduction in the preparation (1 mm and 4 mm) for ceramic veneers presented different fracture resistance values, and smaller incisal reductions reached higher fracture load values.eng
dc.description.provenanceSubmitted by Jakeline Ortega (jakortega@unoeste.br) on 2019-10-15T19:03:00Z No. of bitstreams: 2 license_rdf: 0 bytes, checksum: d41d8cd98f00b204e9800998ecf8427e (MD5) Andressa Restani Oliveira.pdf: 2649486 bytes, checksum: 71cd46bf24723fe1b780dbfdc93aa303 (MD5)eng
dc.description.provenanceMade available in DSpace on 2019-10-15T19:03:00Z (GMT). No. of bitstreams: 2 license_rdf: 0 bytes, checksum: d41d8cd98f00b204e9800998ecf8427e (MD5) Andressa Restani Oliveira.pdf: 2649486 bytes, checksum: 71cd46bf24723fe1b780dbfdc93aa303 (MD5) Previous issue date: 2019-08-29eng
dc.description.sponsorshipCoordenação de Aperfeiçoamento de Pessoal de Nível Superior - CAPESpor
dc.formatapplication/pdf*
dc.thumbnail.urlhttp://bdtd.unoeste.br:8080/jspui/retrieve/3370/Andressa%20Restani%20Oliveira.pdf.jpg*
dc.languageporpor
dc.publisherUniversidade do Oeste Paulistapor
dc.publisher.departmentMestrado em Odontologiapor
dc.publisher.countryBrasilpor
dc.publisher.initialsUNOESTEpor
dc.publisher.programMestrado em Odontologiapor
dc.rightsAcesso Abertopor
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/4.0/-
dc.subjectLaminados Cerâmicospor
dc.subjectRedução Incisalpor
dc.subjectTensão Residualpor
dc.subjectRugosidadepor
dc.subjectCarga de Fratura.por
dc.subjectCeramic Veneerseng
dc.subjectIncisal Reductioneng
dc.subjectResidual Stresspor
dc.subjectSurface Roughnesspor
dc.subjectFracture Resistancepor
dc.subject.cnpqCIENCIAS DA SAUDE::ODONTOLOGIApor
dc.titleCaracterização topográfica e mecânica de laminados cerâmicos com diferentes reduçōes incisais.por
dc.title.alternativeTopographic and mechanical characterization of ceramic veneers with different incisal reductionseng
dc.typeDissertaçãopor
Aparece nas coleções:Mestrado em Odontologia

Arquivos associados a este item:
Arquivo Descrição TamanhoFormato 
Andressa Restani Oliveira.pdfDocumento principal.2,59 MBAdobe PDFThumbnail

Baixar/Abrir Pré-Visualizar


Este item está licenciada sob uma Licença Creative Commons Creative Commons